Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL PPX™ Resin PPX7115 - Americas - (PPE+PP) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL PPX™ Resin PPX7115 - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl PPX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
NORYL PPX™ 7115 resin is a non-reinforced alloy of polyphenylene ether (PPE) + polypropylene (PP). This injection moldable grade exhibits high modulus, high-temperature performance, excellent melt strength, impact resistance, hydrolytic and dimensional stability. NORYL PPX7115 resin is an excellent candidate for applications requiring high modulus and chemical resistance.

UL Yellow Card Link E121562-221243
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 12 cm³/10min ISO 1133
Temperature 260 °C -
Load 5 kg -
ASTM Data
Melt Flow Index, MFI 14 g/10min ASTM D 1238
Temperature 260 °C -
Load 5 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 1370 MPa ISO 527
Yield stress 35 MPa ISO 527
Strain at break 50 % ISO 527
ASTM Data
Tensile Modulus 1240 MPa ASTM D 638
Tensile Strength at Yield 35 MPa ASTM D 638
Tensile Strength at Break 34 MPa ASTM D 638
Elongation at Yield 8 % ASTM D 638
Elongation at Break 125 % ASTM D 638
Flexural Modulus 1370 MPa ASTM D 790
Izod Impact notched, 1/8 in 534 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Vicat softening temperature, A 131 °C ISO 306
Burning behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
ASTM Data
DTUL @ 66 psi 112 °C ASTM D 648
DTUL @ 264 psi 85 °C ASTM D 648
Vicat Temperature 86 °C ASTM D 1525
Other propertiesValueUnitTest Standard
Density 990 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 60 - 65 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 260 - 290 °C -
Mold temperature 30 - 50 °C -
Zone 1 225 - 275 °C -
Zone 2 240 - 280 °C -
Zone 3 250 - 290 °C -
Screw speed 20 - 100 rpm -
Back pressure 0.3 - 0.7 MPa -
Characteristics
Processing
Injection Molding
Regional Availability
North America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.